Patents
US 3,963,631 A#7951114 Most CitedExpiredUnited States (USPTO)Utility

Method of preparing ferroelectric ceramics

12Forward Citations (#7951114 Global)
0.2/yrCitation Velocity (#30232117 Global)
4.87Citation PageRank (#3463616 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for preparing strengthened ferroelectric ceramics, which comprises sintering ceramic materials and then heat treating the sintered ceramics at a temperature from about 100 DEG to about 400 DEG C lower than the final sintering temperature of ceramics, for about 1 to about 60 hrs., and then cooling at a rate from about 300 DEG to about 10 DEG C per hour. Strengthened ferroelectric ceramics are obtained among the following ferroelectric ceramic compositions:

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a ferroelectric ceramic selected from the group consisting of: I. pb([B 1 ] A Ta 1 -A )O 3 --PbTiO 3 --PbZrO 3 , where [B 1 ] is one member selected from the group consisting of Mg, Zn, Cd, Sn, Mn, Fe, Co and Ni when A=1/3, and [B 1 ] is one member selected from the group consisting of Li and Cu when A=1/4, Ii. pb([B 2 ] B Ta 1 -B )O 3 --Pb[B 3 ] C Ta 1 -C )O 3 --PbTiO 3 --PbZrO 3 , where each of [B 2 ] and [B 3 ], [B 2 ]≠[B 3 ], is one member selected from the group consisting of Mg, Zn, Cd, Sn, Mn, Fe, Co and Ni for when B and C=1/3, and each of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗