Process for electroforming nickel foils
Abstract
A method for electroforming relatively smooth seamless nickel, cobalt or nickel-cobalt alloy foil cylinders from an electrolyte for nickel or cobalt is provided comprising slowly increasing the current density from zero to its ultimate current density at the start up of the plating cycle.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 23.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method of electroforming a smooth surface of nickel cobalt or alloy thereof on a conductive substrate from which it may subsequently be removed from a nickel sulfamate electroforming solution, the improvement comprising increasing the current density from zero at an average rate of between about 75 to 600 ASF per minute over the first 2 to 20 percent of the plating cycle to an ultimate current density of between about 200 and about 600 ASF, and the ultimate current concentration is between about 5 and about 15 amperes per gallon of electroforming solution.
- Claim 2Depends on #1
The method of claim 1 wherein the current density is increased at an average rate of between about 100 and about 400 ASF per minute to the ultimate current density.
- Claim 3Depends on #1
The method of claim 1 wherein the electrolyte contains total nickel of from about 12
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗