Abstract

A method is described for the oxidation-leaching of chalcopyrite concentrates at high temperatures and pressures for the extraction of copper values as copper sulfate in which temperatures are maintained between about 425° and 450°F, oxygen partial pressures of between about 50 and 200 psi are provided, and levels of acidity are permitted to increase above about 50 grams of H 2 SO 4 per liter in order to obtain maximum rates of extraction of virtually all of the copper. Thereafter, while maintaining the temperature and pressure at elevated levels, the acidity of the slurry is reduced to between about 10 and 40 grams of H 2 SO 4 per liter in order to obtain reduction of dissolved iron to optimal levels. The resulting slurry is then cooled and further processed for the production of a very pure copper sulfate solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 39.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the oxidation-leaching of chalcopyrite to produce a leach liquor containing at least about 87% of the copper in the chalcopyrite but less than 1.5 grams of iron per liter, comprising: introducing an aqueous slurry of chalcopyrite ore concentrate into an autoclave; treating, for approximately 5 to 15 minutes, the slurry in said autoclave at a temperature of about 425° to 450°F. and at an oxygen partial pressure of about 50 to 200 pounds per square inch while increasing the acid concentration of the slurry to a value in excess of about 50 grams of H 2 SO 4 per liter until at le

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 39 total)

PatentTitleYearCitations
FR 2,483,954 A1Copper sulphate recovery from sulphide material - esp. matte from lead de-coppering by oxidative sulphuric acid leaching—0
US 2004146439 A1Method for recovering metal values from metal-containing materials using high temperature pressure leaching—0
US 11,118,244 B2Low acidity, low solids pressure oxidative leaching of sulphidic feeds20210
US 2005109163 A1Process for multiple stage direct electrowinning of copper—4
US 10,544,482 B2Recovery of copper from arsenic-containing process feed20202
US 2005126923 A1Process for recovery of copper from copper-bearing material using medium temperature pressure leaching, direct electrowinning and solvent/solution extraction—15
US 6,893,482 B2Method for improving metals recovery using high temperature pressure leaching200510
US 2005155458 A1Method for Improving Metals Recovery Using High Temperature Pressure Leaching—0
US 5,902,474 AChloride assisted hydrometallurgical extraction of metal199950
US 7,125,436 B2Method for improving metals recovery using high temperature pressure leaching20068
EP 1,303,640 B1Processing elemental sulfur-bearing materials using high temperature pressure leaching for sulfuric acid production and metal recovery20041
US 2004146438 A1Method for recovery of metals from metal-containing materials using medium temperature pressure leaching—6
US 7,736,487 B2Process for recovery of copper from copper-bearing material using pressure leaching, direct electrowinning and solution extraction20106
US 7,473,413 B2Method for recovering metal values from metal-containing materials using high temperature pressure leaching20095
US 6,676,909 B2Method for recovery of metals from metal-containing materials using medium temperature pressure leaching200412

Non-Patent Literature (1)

  • Evans et al., Editors, International Symposium on Hydrometallurgy AIME, New York, 1973, pp. 375-402.