A process for the manufacture of magnetic materials containing a phase A with a ferromagnetic spin system, of composition Co x Ni 1 -x and a phase B with an antiferromagnetic spin system of composition (CoO) x (NiO) 1 -x , with values of x from 0.05 to 0.96, the phases A and B showing exchange interaction. The materials are manufactured by surface oxidation of starting materials having a ferromagnetic layer, at least on the surface but optionally extending deeper, of composition A, to produce the antiferromagnetic phase B, nitrous oxide being used as the oxidant. Magnetic materials thus obtained have an asymmetrical hysteresis loop, which manifests itself at different temperatures, namely the particular Neel temperature of the phase B, which depends on the composition of the phases which varies in accordance with the values of x.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the manufacture of magnetic pigments exhibiting exchange anisotropy and consisting essentially of two-phase magnetic single-domain particles with the alloy [Co x Ni 1 -x ] as a ferromagnetic phase A and its oxidized form [(CoO) x (NiO) 1 -x ] as an antiferromagnetic phase B, x being from 0.04 to 0.96, which comprises: heating said alloy [Co x Ni 1 -x ] in particulate form at temperatures up to 450°C in the presence of gaseous nitrous oxide (N 2 O) to oxidize the surface of the particles to a depth of from 40 to 1000A to the antiferromagnetic phase B[(CoO) x (NiO) 1

  2. Claim 2Depends on #1

    A process as set forth in claim 1 wherein said temperature is from 40° to 400°C.

  3. Claim 3Depends on #2

    A process as set forth in claim 2 wherein nitrous oxide is mixed with inert gases.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 16 total)

PatentTitleYearCitations
US 7,571,814 B2Method for separating metal values by exposing to microwave/millimeter wave energy20095
CN 115,894,050 ALow-temperature roasting method for producing manganese-zinc ferrite composite material by wet method—5
US 2006248945 A1Method and apparatus for improved determination of spatial non-agglomerated magnetic particle distribution in an area of examination—17
US 2009117355 A1Ultrathin ferromagnetic/antiferromagnetic coupling film structure and fabrication method thereof—0
CN 115,894,050 BLow-temperature roasting method for producing manganese-zinc ferrite composite material by wet method20230
US 7,897,200 B2Ultrathin ferromagnetic/antiferromagnetic coupling film structure and fabrication method thereof20110
DE 2,950,174 A1Verfahren und vorrichtung zur echtheitspruefung von aufzeichnungstraegern, die gegen faelschung zu sichern sind—0
US 4,396,886 ADocument authentication by means of exchange-anisotropic magnetic material198313
US 5,219,554 AHydrated biodegradable superparamagnetic metal oxides199339
US 4,438,462 ADocument identification employing exchange-anisotropic magnetic material19845
US 5,069,216 ASilanized biodegradable super paramagnetic metal oxides as contrast agents for imaging the gastrointestinal tract199163
DE 2,950,129 A1Verfahren und vorrichtung zur echtheitspruefung von aufzeichnungstraegern, die gegen faelschung zu sichern sind—0
US 2009267275 A1Method and Apparatus for Separating Metal Values—6
US 4,314,594 AReducing magnetic hysteresis losses in cores of thin tapes of soft magnetic amorphous metal alloys198234
US 8,469,196 B2Method and apparatus for separating metal values20134