Molten glass is poured on to a bath of molten metal to form a pool of molten glass on the bath, which pool is held back on the bath surface by a solid member, preferably wetted by the glass, extending across the downstream end of the pool. A ribbon of glass is drawn from a forward flow of molten glass beneath the solid member and the ribbon is rapidly cooled to stabilize its dimensions as it is drawn away from the solid member. The method is suitable for the production of flat glass of thickness in the range 0.5 mm to 10 mm; also the production of glass foil of thickness in the range 0.005 mm to 0.5 mm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 19.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing flat glass comprising: providing a forward flow of molten glass along a molten metal surface; defining an elongated aperture for said forward flow of molten glass along said molten metal surface, the molten metal surface defining the lower surface of the aperture and the upper surface of the aperture being of a refractory material wetted by the molten glass and located at a distance above said molten metal surface defining the height of said elongated aperture; drawing a ribbon of glass along the molten metal surface from the flow of molten glass along the molten

  2. Claim 2Depends on #1

    A method according to claim 1, comprising controlling the width of the ribbon by applyin