Abstract

For the preparation of basic aluminum chlorides by reaction of AlCl 3 with aluminum hydroxides, there are generally used aluminum hydroxides easily soluble in mineral acids. According to the process of the invention, however, also such aluminum hydroxides which are soluble in mineral acids only at temperatures above 80°C and which moreover are very cheap may be used when they are reacted with aluminum chloride hexahydrate suspensions at a temperature of from 110° to 150°C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 19.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of aqueous solutions of basic aluminum chlorides of the formula Al 2 (OH) n Cl z , where 0<n<4 and 6>z>2, n + z being always 6, by reaction of hydrochloric acid with an aluminum hydroxide, which comprises preparing in a first step at a temperature of from 80° to 120° C an AlCl 3 .sup.. 6 H 2 O suspension having a concentration in the range of from 278 to 385 milligrams of chloride per gram suspension, from 36 - 55 weight % hydrochloric acid and the equimolar amount of an aluminum hydroxide or hydrated aluminum oxide of such a kind which is soluble i

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • J. W. Mellor's "A Comprehensive Treatise on Inorganic and Theoretical Chemistry," Vol. 5, 1924, p. 318, Longmans, Green & Co., N. Y.