Method for producing high-strength cold rolled steel sheet
Abstract
A method for producing a high-strength cold rolled steel sheet or strip is disclosed. Steel comprising 0.05 to 0.15% of C; 0.02 to 0.30% of Si; 0.10 to 1.5% of Mn; 0.02 to 0.07% of Al; and A total of 0.02 to 0.15% of at least one of Nb, V, Ti and Zr; With the remainder being iron and unavoidable impurities, Is hot rolled whereafter the hot rolled steel sheet or strip is coiled at a temperature of not more than 750°C. The coiled sheet or strip is then cold rolled whereafter the cold rolled steel sheet or strip is subjected to annealing at a temperature between 670°C and 900°C for 20 seconds to 10 minutes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing a high-strength cold rolled steel sheet or strip which comprises: hot rolling steel comprising 0.05 to 0.05% of C; 0.02 to 0.30% of Si; 0.10 to 1.5% of Mn; 0.02 to 0.07% of Al; and a total of 0.02 to 0.15% of at least one metal selected from the group consisting of Nb, V, Ti, and Zr; with the remainder being iron and unavoidable impurities; coiling the hot rolled steel sheet or strip at a temperature not exceeding 750°C. cold rolling the hot rolled steel sheet or strip; subjecting the cold rolled steel sheet or strip to annealing at a temperature betwee
- Claim 2Depends on #1
A method according to claim 1, wherein the coiling is effected at a temperature between 550°C to 750°C.
- Claim 3Depends on #1
A method according to claim 1 in which the annealing is conducted at a temperature between