Abstract

A colored oxide film on the surface of aluminium or an alloy thereof can be formed by anodizing at a D.C. voltage in an electrolyte based on sulfuric acid, followed by alternating current electrolysis at an A.C. voltage which is lower than the D.C. voltage. In order to increase the degree of coloring of the colored oxide film, after the alternating current electrolysis the A.C. voltage is raised to a higher level but lower than the D.C. voltage, followed by dropping the voltage down to a level of the A.C. voltage or thereabout.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process of forming a colored oxide film on a substrate of aluminium or an aluminium alloy, which comprises subjecting the substrate to anodizing at a direct-current voltage E 1 of 10 to 20 volts in an electrolyte comprising an aqueous solution of 4 to 15% by weight of sulfuric acid to form a substantially colorless oxide film on the surface of the substrate, then dropping the voltage E 1 to zero and subjecting the substrate carrying the oxide film on its surface to electrolytic treatment in the same electrolyte by applying an alternating-current voltage E 2 of 2 to 4 volts for a period of

  2. Claim 2Depends on #1

    A process as claimed in claim 1, which further comprises raising the voltage E 2 to a higher voltage E 3 in the range 5 to 10 volts and suddenly d

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗