Method of producing special cokes
Abstract
A method of making special cokes according to which a mixture of from 50-90% by weight of an atmospheric distillation residue of a petroleum, e.g. a Pannonian petroleum, with a density of from 0.935-0.965 grams per cubic centimeter, a viscosity of from 2.8°-4.3° Engler at 100°C, a sulfur content of from 0.85-1.10%, a coke value according to Conradson of from 5-7 %, an aromatics content of from 40-60%, an asphalt content below 1.8% with a boiling component of less than 20% within the temperature range of from 250°-350°C, and a content in ash forming elements of less than 0.05% is coked together with from 10-50% by weight of a catalyst-free catalytic residue obtained by catalytic cracking of a distillate low in ashes, e.g. gas oil, which last mentioned residue has a density of from 0.90-0.95 grams per cubic centimeter, a viscosity of from 2.5°-3.2° Engler at 50°C, a sulfur content less than 0.6%, a coke value according to Conradson of from 3.5-4.5%, an aromatics content of more than 35%, an asphalt content of less than 0.6%, and boiling components of from 8 to 12% for the range of from 250°-300°C and from 30-40% within the temperature range of from 300°-350°C in a 24 to 48 hour cycle
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing cokes for use in connection with the making of ultra-high-power electrodes which includes in combination the steps of: coking a mixture of from 50 to 90% by weight of atmospheric virgin reduced crude oil having a density of from 0.935 to 0.965 grams per cubic centimeter, a viscosity of from 2.8° to 4.3° Engler at 100°C, a sulfur content of from 0.85 to 1.10%, a coke value according to Conradson of from 5 to 7%, a content in aromatics of from 40 to 60%, an asphalt content below 1.8% with a boiling component less than 20% within the temperature range of from 250° to 350°C,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗