Patents
US 3,923,924 A#15188724 Most CitedExpiredUnited States (USPTO)Utility

Antistatic fiber containing chain-extended tetrols based on diamines

7Forward Citations (#15188724 Global)
0.1/yrCitation Velocity (#39230022 Global)
1.79Citation PageRank (#17320183 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

It has been suggested that antistatic properties of fibers of polyamide could be improved by uniformly dispersing in the polyamide between about 1 percent and about 12 percent by weight of a predominantly branched, chain-extended propylene oxideethylene oxide copolymer based on a diamine. However, with incorporation of this antistatic additive in the polyamide, serious problems have been encountered in melt-spinning due to the frequent occurrence of ''''nubs'''' or enlarged places in the extruded polyamide filament. It has now been found that the occurrence of said nubs in the antistatic polyamide fiber can be greatly reduced by dispersing in the polymer about 0.5 to 12% by weight, based on the weight of the antistatic agent, of a phenol compound represented by the formula: In comparative tests with antistatic yarns containing various commercially available hindered phenol compounds, the yarns of the present invention showed significantly greater breaking strength retention after exposure to light in standard tests.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    IN A PROCESS FOR THE FORMATION OF AN ANTISTATIC POLYAMIDE FIBER FROM A FIBER-FORMING POLYAMIDE POLYMER CONTAINING ABOUT 1% TO 12% BY WEIGHT OF AN ANTISTATIC COMPOUND WHICH IS A CHAIN-EXTENDED REACTION PRODUCT OF A TETROL COMPOUND REPRESENTED BY THE FORMULA:

  2. Claim 2Depends on #1

    The process of claim 1 wherein the ethylene oxide moieties make up about 10% to about 90% of the molecular weight of the tetrol compound and the chain-extended antistatic compound has a melt viscosity of about 800 to 50,000 centipoises at 100*C.

  3. Claim 3Depends on #2

    The process of claim 2 wherein the phenol compound is selected from the group consisting of 4,4''-butylidene bis-(6-tert. butyl m-cresol); 4,4''-butylidene bis-(6-tert. amyl m-cresol); and 4,4''-heptylidene bis-(6-tert. butyl m-cresol).

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗