Abstract

Process for extracting cobalt and nickel from oxidized nickel ores containing between 0.5-5% w/w nickel, 5-30% w/w iron, 1.025% w/w magnesium and minor amounts of cobalt which process comprising firstly selectively reducing the ore so that substantially all the nickel and cobalt values are reduced to metal but substantially all the iron remains as oxide; secondly, treating the reduced ore with a mixture of hydrogen chloride and steam at a temperature in the range 150 to 500*C and at a volume ratio of steam to hydrogen chloride in the range 1:2 to 15:1 preferably 2:1 to 12:1 and, thirdly, leaching the nickel and cobalt values from the reduced ore with an aqueous leaching solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A PROCESS FOR EXTRACTING COBALT AND NICKEL FROM OXIDIZED NICKEL ORES CONTAINING BETWEEN 0.5-5% NICKEL, 5-30% IRON, 1.0-25% W/W MAGNESIUM AND MINOR AMOUNTS OF COBALT, WHICH PROCESS COMPRISES FIRSTLY, SELECTIVELY TREATING THE ORE WITH A REDUCING AGENT UNDER REDUCING CONDITIONS SO THAT SUBSTANTIALLY ALL THE NICKEL AND COBALT VALUES ARE REDUCED TO METAL BUT SUBSTANTIALLY ALL THE IRON AND MAGNESIUM REMAIN AS OXIDE SECONDLY, TREATING THE REDUCED ORE WITH A MIXTURE OF HYDROGEN CHLORIDE AND STEAM AT A TEMPERATURE IN THE RANGE FROM 150* TO 500*C AND AT A VOLUME RATIO OF STEAM TO HYDROGEN CHLORIDE IN TH