Nitrided boron steel
Abstract
A method of economically producing steel parts having high case hardness and commensurate core properties, the parts being formed from low carbon steel containing about 0.25 to 0.50 percent of carbon, about 0.80 to 1.60 percent of manganese, about 0.40 maximum percent of silicon, about 0.0003 to 0.005 percent of boron, up to approximately 0.1 percent of a suitable nitriding agent such as vanadium, titanium tungsten, aluminum, zirconium, columbium, chromium or molybdenum, balance essentially iron, the boron and nitriding agent being in an uncombined or atomic form, the parts being hardened to develop desirable core properties and then being nitrided to develop case hardness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 9.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD OF ECONOMICALLY PRODUCING STEEL PARTS HAVING HIGH CASE HARDNESS AND COMMENSURATE CORE PROPERTIES, COMPRISING THE STEPS OF FORMING THE STEEL PARTS FROM STEEL CONSISTING OF ABOUT 0.25 TO 0.50 PERCENT OF CARBON ABOUT 0.8 TO 1.60 PERCENT OF MANGANSESE, NORMAL IMPURITIES, ABOUT 0.0003 TO 0.005 PERCENT OF BORON, APPROXIMATELY 0.03 TO 0.05 PERCENT VANDIUM AS A NITRIDING AGENT, AND THE BALANCE IRON, THE BORON AND VANADIUM BEING PRESENT IN UNCOMBINED FORM, PRELIMINARILY HARDENING THE PARTS TO DEVELOP CORE TOUGHNESS, BEAM STRENGTH AND DEPTH HARDNESS, AND NITRIDING THE STEEL PARTS TO FORM A CASE
- Claim 2Independent Claim
Steel parts having high case hardness and commensurate core properties of core toughness, beam strength and depth hardness, the parts being produced by the steps of forming the p