Plastic plating process and solution therefor

7Forward Citations (#14899023 Global)
0.1/yrCitation Velocity (#39201326 Global)
1.95Citation PageRank (#15182096 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process for the plating of a non-metallic material, such as polyethylene or polypropylene strip, which includes the step of immersing said material in an alcohol solution containing boron, phosphorous and a metal selected from the group consisting of gold, palladium, rhodium and platinum. The metal film forms adherently on the strip. The solution is prepared by mixing phosphorous pentoxide in an alcohol solvent. The dissolution of the phosphorous pentoxide is exothermic and the temperature of the solution will rise during the reaction. Then, boric anhydride and a salt of gold, palladium, rhodium or platinum is added. The solution appears to strip any contamination while depositing a layer of the gold, platinum, rhodium or palladium onto the surface of the non-metallic part. The process is particularly advantageous for preparing metallized strips for use during semiconductor device assembly.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A PROCESS OF PLATING NON-METALLIC MATERIAL WHICH CONSISTIS OF THE STEP OF COATING THE MATERIAL WITH A COMPLEX SOLUTION CONSISTING ESSENTIALLY OF 1 TO 30 GRAMS PER LITER PHOSPHOROUS PENTOXIDE, 1 TO 60 GRAMS PER LITER BORIC ANHYDRIDE, 0.01 TO 10.0 GRAMS PER LITER OF A MATERIAL SELECTED FROM THE GROUP CONSISTING OF GOLD, PLATINUM, PALLADIUM AND RHODIUM SALTS AND OXIDE, AND THE BALANCE A SOLVENT SELECTED FROM THE GROUP CONSISTING OF METHYL, ETHYL, PROPYL, ISOPROPYL, BUTYL, AND ISOBUTYL ALCOHOL, ETHYLENE GLYCOL, AND TETRAHYDRO FURFURYL ALCOHOL.

  2. Claim 2Depends on #1

    In a process as recited in claim 1 wherein said coating step includes immersing a semiconductor device in said complex solution for 1 - 24 hours at room temperature.

  3. Claim 3Depends on #1

    In a process as recited in claim 1 wherein said coating step includes covering a surface of a semiconductor device with said complex soluti

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗