Method of producing synthetic cis-1,4-polyisoprene rubber having high green strength
Abstract
A reaction between synthetic cis-1,4-polyisoprene rubber and maleic anhydride in solution is carried out in the presence of at least 10 moles of isoprene monomer per mole of maleic anhydride using a free radical initiator in an amount which is both from 0.02 to 10 moles per mole of maleic anhydride and 0.1 to 15 millimoles per 100 g of the rubber, to produce a modified polyisoprene rubber having an improved green strength with the suppression of gel formation during the reaction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A METHOD OF PRODUCING SYNTHETIC CIS-1,4-POLYISOPRENE RUBBER HAVING AN IMPROVED GREEN STRENGTH, WHICH COMPRISES REACTING SYNTHETIC CIX-1,4-POLYISOPRENE WITH MALEIC ANHYDRIDE IN, AS AN INERT REACTION MEDIUM, AN AROMATIC HYDROCARBON SOLVENT OR A SATURATED ALIPHATIC HYDROCARBON SOLVENT FOR SAID POLYISOPRENE IN THE PRESENCE OF ISOPRENE MONOMER IN AN AMOUNT OF AT LEAST 10 MOLES PER MOLE OF MALEIC ANHYDRIDE AND ALSO IN THET PRESENCE OF A FREE RADICAL INITIATOR IN AN AMOUNT WHICH IS BOTH FROM 0.02 TO 10 MOLES PER MOLE OF MALEIC ANHYDRIDE AND FROM 0.1 TO 15 MILLIMOLES PER 100 G OF SAID POLYISOPRENE RUB
- Claim 2Depends on #1
The method of claim 1, wherein the maleic anhydride is present in an amount of from 0.1 to 10 parts by weight per 100 parts by weight of the rubber.
- Claim 3Depends on #1
The method of claim 1, wherein the reaction is carried out until synthetic cis-1,4-polyisoprene h
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,567,691 A | Maleinization of synthetic rubber | 1971 | 19 |
| US 3,651,025 A | Diene polymerization process | 1972 | 16 |
| US 3,778,418 A | Maleinization process | 1973 | 34 |