Wellbore oxidation of lixiviants
Abstract
Recovery of metal values such as copper values from a wellbore is combined with the pregnant liquor treatment to achieve as part of the recovery operation the pregnant liquor processing; during a gas-lift operation of the pregnant liquor ferrous ions in the pregnant liquor are being oxidized and a suitable lixiviant is obtained for reintroduction in the wellbore; as an embodiment of the invention sulfur dioxide augmented oxygen containing gas is used for treating the pregnant liquor to aid the oxidation and generate sulfuric acid being used up during the copper value recovery.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
IN A PROCESS FOR IN-SITU MINING OF MINERALS CONTAINING METAL VALUES SUCH AS COPPER VALUES WHEREBY A LIXIVIANT IS INTRODUCED INTO AT LEAST ONE WELLBORE AND A PREGNANT LIQUOR REMOVED THEREFROM, THE COMBINATION COMPRISING: INTRODUCING IN A WELLBORE A GAS-LIFT COMPRISING FROM 4 TO 11 SCF OF AIR PER GALLON OF PREGNANT LIQUOR LIFTED PER 1000 FT., MAINTAINING IN SAID GAS-LIFT DURING SAID LIFT OXYGEN, LIFTING THE PREGNANT LIQUO 5 MINUTES TO 2 HOURS WHEREBY THE RATE OF OXIDATION OF FERROUS AT A RATE SUCH THAT THE RESIDENCE TIME IN THE WELLBORE IS ABOUT IONS IN SAID PREGNANT LIQUOR IS SUCH THAT NEARLY 1
- Claim 2Independent Claim
The
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗