Production of elastic yarn
Abstract
The present invention relates to a process for preparing elastic filament for yarn with improved breaking strength and elastic recovery. The process comprises preparing a composition by adding 0.1 to 1 part of a fatty acid amine, fatty acid methylol amide or higher fatty acid ester to 100 parts of a polytetramethylene glycol-polyethylene terephthalate block copolymer of an inherent viscosity of more than 2.0 obtained from polytetramethylene glycol and polyethylene terephthalate, melt-spinning the composition to form filaments and stretching, then shrinking the formed filaments while heating them.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR PRODUCING ELASTIC FILAMENTS WHEREIN: A COMPOSITION PREPARED BY ADDING A. 5 TO 15 PARTS OF OLIGOMER OF STYRENE, A-METHYL STYRENE OR VINYL TOLUENE OR A COPOLYMERIZED OLIGOMER THEREOF OF MOLECULAR WEIGHT OF 300 TO 1,000 AND B. 0.1 TO 1 PART OF A FATTY ACID AMIDE, FATTY ACID METHYOL AMIDE OR HIGHER FATTY ACID ESTER TO C. 100 PARTS OF A POLYTETRAMETHYLENE GLYCOPOLYETHYLENE TEREPHTHALATE BLOCK COPOLYMER OF AN INHERENT VISCOSITY OF MORE THAN 2.0 OBTAINED FROM POLYTETRAMETHYLENE GLYCOL HAVING A MOLECULAR WEIGHT OF 1800 TO 200 AND POLYETHYLENE TEREPHTHALATE THE CONTENT OF WHICH IN THE COP
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,023,192 A | Segmented copolyetherester elastomers | 1962 | 156 |
| US 3,651,014 A | Segmented thermoplastic copolyester elastomers | 1972 | 309 |
| US 3,660,557 A | Polyester product | 1972 | 8 |
| US 3,701,755 A | Production of elastomers | 1972 | 43 |