Method of treating coal mining refuse

30Forward Citations (#2209396 Global)
0.6/yrCitation Velocity (#13492668 Global)
15.89Citation PageRank (#490302 Global)
1Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Sulfuric acid-containing coal mining refuse is reacted in the presence of moisture with lime, and preferably also with a pozzolanically active material such as fly ash, whereby the existing sulfuric acid is neutralized with lime and further reacted with lime and pozzolan to produce a non-polluting cementitious material, which is self-hardening at atmospheric pressure. This material may be used as structural fill or as a road base material. Alternatively, piles of such refuse may be treated so that a self-hardening mixture is formed either totally or on the surface thereof, thereby preventing further water percolation therethrough and resultant subsurface water contamination.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 30.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method of treating sulfuric acid-containing coal mining refuse comprising intimately admixing said refuse, in the presence of water, with lime, the amount of lime exceeding that stoichiometrically necessary to neutralize said sulfuric acid content of said refuse, and permitting said admixture to harden, at atmospheric pressure, for at least several days.

  2. Claim 2Depends on #1

    Method of treating mining refuse, as recited in claim 1, wherein pozzolanically active particulate material is concurrently intimately a