Method of processing steel material having high austenitic grain-coarsening temperature

2Forward Citations (#34477494 Global)
0.0/yrCitation Velocity (#55110407 Global)
1.81Citation PageRank (#17053718 Global)
1Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of processing steel material having a high austenitic grain-coarsening temperature and an abnormal grain growth curve of cold worked austenitic grain, which comprises heating said steel material at a temperature of from the ferrite recrystallization temperature to the A1 transformation point for more than five minutes to cause recrystallization. This technique prevents the formation of mixed grains upon austenitizing and thereby preserves the mechanical properties of the steel material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A METHOD OF PROCESSING STEEL MATERIAL WHICH IS CHARACTERIZED BY AN ABNORMAL GRAIN GROWTH CURVE OF AUSTENITIC GRAIN AFTER COLD WORKING AND WHICH HAS A HIGH GRAIN COARSENING TEMPERATURE WHICH COMPRISES: HEATING SAID COLD WORKING STEEL MATERIAL TO A TEMPERATURE OF BETWEEN THE FERRITE RECRYSTALLIZATION TEMPERATURE AND THE A1 TRANSFORMATION TEMPERATURE FOR A PERIOD OF AT LEAST 5 MINUTES SO AS TO EFFECT RECRYSTALLIZATION OF THE FERRITIC STRUCTURE WHICH HAD BECOME DEFINED DURING COLD WORKING, AND THEREBY RESING THE AUSTENITIC GRAIN COARSENING TEMPERATURE, FURTHER HEATING SAID STEEL MATERIAL TO A TEMP

  2. Claim 2Independent Claim

    A method of processing steel material which contains a grain refining element which is