Method of processing ferroelectric devitrifiable glass ceramics
Abstract
The electrical properties of ferroelectric devitrifiable glass ceramics are improved by subjecting the ceramics to inert gas pressures of about 5,000 pounds per square inch to about 50,000 pounds per square inch at temperatures from about 700* C. to about 1,100* C. for about 15 minutes to about 2 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 11.
Claims (2 — 0 Independent, 2 Dependent)
- Claim 2Depends on #1
Method according to claim 1 wherein the ferroelectric devitrifiable glass ceramic is barium strontium niobate devitrifiable glass ceramic, the temperature is about 775*C., and the inert gas pressure is about 10,000 to about 30,000 pounds per square inch of helium; the devitrified body so obtained being characterized by a dielectric constant of 380, a dielectric strength of up to 3,000 volts per mil, a dissipation factor below 0.25 percent, and a more stable coefficient of dielectric constant under DC stress that is improved from a 20 percent change at 500 volts per mil to only a 14 percent cHa
- Claim 3Depends on #1
Method according to claim 1 wherein the ferroelectric devitrifiable glass ceramic is barium strontium titanate devitrifiable glass ceramic, the temperature is about 900* C., and the inert gas pressure is about 10,000 to about 30,000 pounds per squa
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗