Abstract

The preparation of a smokable material in which a cellulosic material containing a metal salt in the form of the carbonate, oxalate pivalate or glycolate of calcium or magnesium or other alkaline earth metals and mixtures thereof and a metal salt in the form of chloride or sulfate of the metal is subjected to thermal degradation in a non-oxidizing atmosphere at a temperature within the range of 270*-500*C for a time sufficient to effect a weight loss within the range of 40-75 percent and which includes modifying the thermally degraded cellulosic material by the addition of a binder in an amount within the range of 0.5-10 percent by weight and materials for strengthening and flexibilizing the cellulosic material prior to degradation, including a starch, sugar and dextrin and mixtures thereof, plus additives to improve color, taste, aroma and moisture retention characteristics.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 18.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A smokable material as claimed in claim 1 in which the cellulosic material has been exposed to the thermal reaction temperature for a time sufficient to effect a weight loss within the range of 50-60 percent.

  2. Claim 3Depends on #1

    A smokable material as claimed in claim 1 in which the compound is selected from the group consisting of the oxalate and carbonate of calcium and magnesium.

  3. Claim 4Depends on #3

    A smokable material as claimed in claim 3 in which the carbonate and/or oxalate of the alkaline earth metal is present in an amount within the range of 15-20 percent by weight.