Method for the manufacture of carbon foam
Abstract
Carbon foam is produced by admixing a thixotropic binder of partially polymerized furfuryl alcohol containing less than 12 mole per cent free alcohol with water and a two-component urethane system comprising a resin of polyhydric alcohol and diisocyanate for providing a structure of foam which is then cured and subsequentially heated to a temperature sufficient to thermally decompose the urethane and carbonize the binder. The preparation of a multi-batch quantity of the above admixture is accomplished by premixing the foam forming components except for the diisocyanate into a homogeneous premix while shearing the binder to reduce the viscosity of the premix to facilitate the handling and mixing thereof and heating this premix during the preparation thereof to a temperature in the range of about 35* to 40*C. to inhibit coagulation. A selected quantity of the premix is then mixed with the diisocyanate component and poured into a suitable mold.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
IN THE ART OF PREPARING A CELLULAR CARBONACEOUS PRODUCT COMPRISING THE STEPS OF ADMIXING PARTIALLY POLYMERIZED FURFURYL ALCOHOL CONTAINING LESS THAN 12 MOLE PER CENT OF THE ALCOHOL MONOMER AND POSESSING A VISCOSITY IN THE RANGE OF ABOUT 10,000 TO 14,000 CENTIPOISE WITH WATER AND URETHANE COMPOUNDS CAPABLE OF INTERACTING TO FORM A CELLULAR URETHANE STRUCTURE AND CONSISTING ESSENTIALLY OF A POLYHYDRIC URETHANE AND DIISOCYANATE FORMING A CELLULAR URETHANE STRUCTURE BY THE INERACTION OF THE URETHANE COMPOUNDS, HEATING THE CELLULAR URETHANE STRUCTURE TO A TEMPERATURE BELOW THE DECOMPOSITION TEMPERA
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗