Method for preparing scandium metal
Abstract
1. A PROCESS FOR PREAPRING HIGH-PURITY SCANDIUM METAL FROM SCANDIUM OXIDE COMPRISING: (A) FIRING THE SCANDIUM OXIDE AT 650 TO 750*C., RESIDUAL VOLATILE MATERIALS AND ANY CARBON PRESENT IN SAID OXIDE; (B) HEATING THE FIRED OXIDE TO 650 TO 750*C., (C) PASSING PHOSGENE GAS OVER THE HEATED OXIDE, THEREBY CHLORINATING THE OXIDE IN A REDUCING ATMOSPHERE CONTAINING NO FREE CARBON TO SCANDIUM CHLORIDE; (D) MIXING THE SCANDIUM CHLORIDE WITH A MEMBER SELECTED FROM THE GROUP CONSISTING OF MAGNESIUM, CALCIUM AND MIXTURES THEREOF TO FORM A CHARGE; (E) HEATING THE CHARGING UNDER REDUCED PRESSURE TO FROM ABOUT 800 TO 1000*C., WHEREBY THE SCANDIUM CHLO- RIDE IS REDUCED TO SCANDIUM METAL; AND (F) RECOVERING THE HIGH-PURITY SCANDIUM METAL.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A PROCESS FOR PREAPRING HIGH-PURITY SCANDIUM METAL FROM SCANDIUM OXIDE COMPRISING: (A) FIRING THE SCANDIUM OXIDE AT 650 TO 750*C., RESIDUAL VOLATILE MATERIALS AND ANY CARBON PRESENT IN SAID OXIDE; (B) HEATING THE FIRED OXIDE TO 650 TO 750*C., (C) PASSING PHOSGENE GAS OVER THE HEATED OXIDE, THEREBY CHLORINATING THE OXIDE IN A REDUCING ATMOSPHERE CONTAINING NO FREE CARBON TO SCANDIUM CHLORIDE; (D) MIXING THE SCANDIUM CHLORIDE WITH A MEMBER SELECTED FROM THE GROUP CONSISTING OF MAGNESIUM, CALCIUM AND MIXTURES THEREOF TO FORM A CHARGE; (E) HEATING THE CHARGING UNDER REDUCED PRESSURE TO FROM ABOUT
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗