Reducing heat-seal temperature requirements for coatings prepared from latexes of vinylidene chloride polymers
Abstract
WHEREIN R1 is hydrogen or alkyl and R2 is alkyl wherein the sum of R1 and R2 equals from eight to 20 carbon atoms; where Y is hydrogen or methyl; where n is an integer from 6 to 40; and where R3 is hydrogen or methyl. A process for reducing the heat-seal temperature requirements of films and coatings produced from high vinylidene chloride polymer latexes comprising having present in films or coatings formed from such latexes, prior to fusion thereof, from about 0.5 to about 5 percent by weight of latex polymer solids of an alkyl phenol olefin oxide adduct of the formula
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 4.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
AT LEAST ABOUT 80 PERCENT BY WEIGHT BASED ON THE TOTAL WEIGHT OF MONOMERS USED OF VINYLIDENE CHLORIDE, AND
- Claim 2Independent Claim
from about 0.1 to about 5 percent based on the total weight of the monomers used of a significantly water-soluble ionic material selected from the group of sulfonic acids and their salts having the formula R-Z-Q-SO3 -M+ wherein the radical R is selected from the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.