Hot pressed, high strength silicon nitride
Abstract
The fabrication of high strength, high density, silicon nitride by the addition of between 1.0 to 3.5 percent by weight of yttrium in the form of a compound to silicon nitride powder and pressing the material at temperatures of between 1,750* C. and 1,800* C. and at uniaxial pressures of between 6,000 and 7,000 psi.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 40.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A composition according to claim 1 in which the yttrium compound is a member of the group consisting of yttrium chloride, yttrium nitrate and yttrium oxide.
- Claim 3Depends on #1
A composition according to claim 1 in which the yttrium compound is yttrium oxide.
- Claim 4Depends on #3
A composition according to claim 3 in which the amount of yttrium oxide is about 1.25 to 4.45 weight percent of the weight of the silicon nitride.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 40 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,108,887 A | Refractory articles and method of making same | 1963 | 81 |