Heat resistant vulcanizable blend of butadiene/styrene rubbers and ethylene propylene-diene terpolymers
Abstract
A sulfur vulcanizable blend having improved properties is obtained by blending from 40 to 60 parts by weight of a solution polymerized copolymer of butadiene and styrene, from 10 to 55 parts by weight of an emulsion polymerized copolymer of butadiene and styrene, from 25 to 45 parts by weight of a termpolymer of ethylene, propylene and a diene comonomer, from 40 to 70 parts by weight of an extender oil per 100 parts by weight of total polymer, and from 120 to 200 parts by weight of carbon black per 100 parts by weight of total polymer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A blend in accordance with claim 1 wherein said solution polymerized copolymer of butadiene and styrene has a butadiene-to-styrene molar ratio in the range of about 73:27 to about 77:23 with no detectable polystyrene.
- Claim 3Depends on #1
A blend in accordance with claim 1 wherein said emulsion polymerized copolymer of butadiene and styrene has a butadiene-to-styrene molar ratio in the range of about 74:26 to about 78: 22.
- Claim 4Depends on #1
A blend in accordance with claim 1 wherein said blend has a compression set (ASTM-D 395-61) of less than 22 and an uncured hardness of at least about 70.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.