Process for producing conjugated diene polymers
Abstract
A conjugated diene polymer having a high cis-1,4 configuration content and having a high molecular weight can advantageously be produced by homopolymerizing or copolymerizing at least one conjugated diene or copolymerizing at least one conjugated diene with at least one vinyl aromatic hydrocarbon with a catalyst consisting essentially of at least one organolithium compound and at least one aliphatic nitrile in a proportion of 0.01 to 1.0 mole of the aliphatic nitrile per carbon-linked lithium atom and optionally carbon disulfide as promoter. The vulcanizate of said polymer of isoprene is very similar in physical properties to that of a natural Hevea rubber.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A process according to claim 1, wherein the amount of the catalyst is 0.01 to 100 milligram equivalent in terms oF carbon-linked lithium per mole of the monomer or monomers.
- Claim 3Depends on #1
A process according to claim 1, wherein the polymerization is effected under a pressure of from atmospheric pressure to 10 atmospheres at a temperature of from -50* C to +100* C.
- Claim 4Depends on #1
A process according to claim 1, wherein the polymerization is effected under an inert atmosphere.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗