Process for fabricating porous beryllium billets
Abstract
Porous beryllium billets are prepared by cold isostactic pressing of a mold containing beryllium powder, and sintering under a vacuum the resulting beryllium billet. The billets so produced are particularly useful as a matrix material for active transpiration systems.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 2Depends on #1
The process according to claim 1 in which the billet is annealed by heatiNg at a temperature of about 1,350* F for about 1 hour.
- Claim 3Depends on #2
The process according to claim 2 in which the billet is sintered under a vacuum at a temperature in the range of 2010 to 2035*F for a period of 2 to 4 hours.
- Claim 4Independent Claim
A porous beryllium billet having a permeability in the range of 1 X 10 10 to 1 X 10 12 in2.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,794,241 A | Fabrication of intricate shapes from beryllium | 1957 | 8 |
| US 2,818,339 A | Method for producing malleable and ductile beryllium bodies | 1957 | 15 |
Non-Patent Literature (1)
- Hausner et al., The Powder Metallurgy of Beryllium ASM 1950 Preprint No. 38