Reduction of nickel oxide in a rotary hearth furnace
Abstract
Briquetted compounds selected from the group consisting of nickel oxide, cobalt oxide and compounds heat decomposable thereto, particularly at temperatures below 1,000*C., are fed to a rotary hearth furnace to form a static shallow bed of briquettes that is heated by radiation and convection to a temperature between about 750*C. and 1,000*C. and is treated with a carbonaceous reductant to reduce the compound to metal. Advantageously, the carbonaceous reductant is incorporated in the briquettes and is a liquid hydrocarbon.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 12.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The process as described in claim 1 wherein the moving hearth is continuous, the metallic briquettes are discharged from the furnace at a temperature of at least about 750*C., and the briquetted compound is fed to the continuous hearth which is at a temperature of at least about 750*C.
- Claim 3Depends on #1
The process as described in claim 1 wherein the liquid hydrocarbon is Bunker C oil.
- Claim 4Depends on #3
The process as described in claim 3 wherein the liquid hydrocarbon is are added to the briquettes in amounts to substantially satisfy the stoichiometry of the reduction reactions.
Technical Overview & Description