Method of toughening glass sheets
Abstract
A glass sheet of thickness in the range 1.8 mm to 4 mm having a dual fracture characteristic is toughened by heating the sheet to a temperature near its softening point, exposing the surface of the hot glass sheet to gaseous chilling medium and maintaining a rate of flow of the gaseous chilling medium dependent on the glass thickness, the rate being just sufficient to give a selected heat transfer coefficient with respect to the glass in the range bounded by from 0.008 to 0.02 calories.cm 2.* C 1.sec 1 for 1.8 mm glass and from 0.006 to 0.009 calories.cm 2.* C 1.sec 1 for 4 mm glass. The central tensile stress thereby induced in the glass is from 260 kg/cm2 to 470 kg/cm2 for 1.8 mm glass reducing to from 210 kg/cm2 to 330 kg/cm2 for 4 mm glass.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 2Independent Claim
* C 1. sec 1 for 3 mm glass, thereby producin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.