Titanium and zirconium diborides are electrolytically synthesized using a molten sodium salt electrolyte containing cryolite, a sodium alkali, a sodium borate, a sodium halide and a source compound to supply the titanium or zirconium. Substantial refining occurs during the synthesis allowing the use of rutile concentrates as a source of titanium and zircon concentrates as a source of zirconium. The synthesis may be accomplished in a cell open to the atmosphere to produce substantially pure titanium and zirconium diborides.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 8.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    The process of claim 1 wherein the electrolyte temperature is maintained within the range of 900* to 1100* during electrolysis.

  2. Claim 3Depends on #2

    The process of claim 2 wherein the sodium alkali is chosen from the group consisting of sodium hydroxide, sodium carbonate, sodium oxide and mixtures thereof.

  3. Claim 4Depends on #3

    The process of claim 3 wherein the sodium borate is chosen from the group consisting of borax, sodium metaborate, sodium orthoborate, sodium diborate, sodium tetraborate, sodium pentaborate and mixtures thereof.