Method of treating a carbon current collection brush and brush resulting therefrom
Abstract
A method of treating a carbon current collection brush for increased high temperature life which comprises contacting at least one surface of the brush with a solution of phosphorus oxychloride and baking the brush at a temperature from 200*C to 700*C thereby reducing the amount of phosphorus oxychloride to 1 to 4 weight percent of the brush weight. A modified method includes the above method steps but includes a pretreatment step in a mild aqueous oxidant, such as, a hypochlorite solution. A carbon current collection brush has a carbon body and the body contains from about 0.1 to 5 weight percent of phosphorus oxychloride.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A method of treating a carbon current collection brush as in claim 1, in which the brush is baked at a temperature in the temperature range of from 400* to 700*C for at least one hour.
- Claim 3Depends on #1
A method of treating a carbon current collection brush as in claim 1, in which the brush is pretreated in a mild aqueous oxidant solution.
- Claim 4Depends on #3
A method of treating a carbon current collection brush as in claim 3, in which the oxidant solution is sodium hypochlorite.