Additive cement compositions and method
Abstract
An additive composition for enhancing the properties of hydraulic cement compositions, and a hydraulic cement composition of enhanced properties, particularly useful in the cementing of wells, and methods of cementing geologic formations traversed by well bores are disclosed. The additive composition comprises a water soluble lignosulfonate or lignosulfonic acid or mixtures thereof, and tartaric acid or a salt of tartaric acid or mixtures thereof, and preferably about 3 parts calcium lignosulfonate and 1 part tartaric acid, although good results are obtained with 1 to 19 parts lignosulfonate or lignosulfonic acid and 19 to 1 parts tartaric acid or a salt of tartaric acid. The hydraulic composition includes a hydraulic cement and preferably about 11/2 % of the additive composition based on the weight of the cement; although , good results are obtained with from about 0.10% to about 3%, or higher, for example, for long life slurries. Especially good results are obtained when the hydraulic cement has been pretreated and aged as in our co-pending application filed Jan. 25, 1971, Ser. No. 109,606. The hydraulic cement composition has good viscosity and strength, ideal thickening times,
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 2Depends on #1
The hydraulic cement composition of claim 1 where the lignosulfonate is calcium lignosulfonate, and the selected member is tartaric acid.
- Claim 3Depends on #1
The hydraulic cement composition of claim 1 where the retarder composition consists essentially of about 3 parts calcium lignosulfonate and about 1 part tartaric acid.
- Claim 4Independent Claim
A hydraulic cement composition consisting of a substantially dry hydraulic cement free of substantial lumping intimately mixed with a small amount of liquid water and aged for a period of at least about 30 minutes, and about 0.10% to at least about 3.00% of a retarder composition based on the weight of the dry cement consisting essentially of from about 1 part to about 19 parts by weight of a member selected from the group consisting of a water soluble lignosulfonate, lignosulfonic acid and mixtures thereof, and from about 1 part to about
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗