Adhesive composition and method of preparation
Abstract
A process for the production of an aqueous emulsion of an ethylene-vinyl acetate polymer is disclosed wherein the polymerization is performed in the presence of a preformed seed emulsion, from 1.5 to 6 weight percent of a protective colloid comprising a mixture of fully and partially hydrolyzed polyvinyl acetate and a minor amount, from 0.01 to 1 weight percent, of an unsaturated acid having from three to six carbon atoms. The seed emulsion is comprised of an aqueous emulsion containing from 25 to 63 weight percent of ethylene-vinyl acetate copolymers having an ethylene content between about 5 and 20 weight percent and from 2 to 6 weight percent of a partially hydrolyzed polyvinyl acetate. The polymerization is performed under an ethylene pressure of from 100 to 1000 psig., sufficient to incorporate from 5 to 20 weight percent ethylene in the final copolymer product and carried out until the total free monomer content of the emulsion is maintained below about 1 weight percent. Conventional free radical initiation of the polymerization reaction is used. The resultant emulsion can be used as an adhesive since films formed therefrom exhibit a high degree of adhesiveness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 33.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The process defined in claim 1 wherein said partially hydrolyzed polyvinyl acetate in said seed emulsion and in said polyvinyl alcohol mixture is about 80 to 95 percent hydrolyzed and exhibits a viscosity of about 2 to 80 centipoises for a 4 weight percent aqueous solution at a temperature of 20*C.
- Claim 3Depends on #1
The process defined in claim 1 wherein said fully hydrolyzed polyvinyl acetate exhibits a viscosity of from about 5 to 125 centipoises for a 4 weight percent aqueous solution at a temperature of 20*C.
- Claim 4Depends on #1
The process defined in claim 1 wherein said weight ratio of fully to partially hydrolyzed polyvinyl alcohol is between about 1 to 5 and 5 to 1.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗