Patents
US 3,768,992 A#37484664 Most CitedExpiredUnited States (USPTO)Utility

Toughening of ophthalmic lens blanks

2Forward Citations (#37484664 Global)
0.0/yrCitation Velocity (#55534558 Global)
1.10Citation PageRank (#36371611 Global)
3Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

Impact resistance of lenses treated according to the invention is increased by quenching in a molten metal under a non-oxidizing or slightly reducing atmosphere.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 2.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    The method according to claim 1 in which the metal is selected from the group consisting essentially of liquid mercury, and the molten metals tin, lead, bismuth, cadmium, gallium, indium, thallium, and low melting alloys of these metals.

  2. Claim 3Depends on #1

    The method of claim 1 wherein the center thickness of said lens is in the range of approximately .6 to .8 millimeter.

  3. Claim 4Depends on #1

    The method of claim 1 including the step of annealing said lens prior to preheating said lens for immersion into said bath.