Method for sintering very pure yttria compacts to transparency
Abstract
Finely divided Yttria having a purity of at least 99.99 percent is pressed into compacts, sintered in dry hydrogen or a partial vacuum to temperatures in the range of 2,150*-2,330*C, and refired in wet hydrogen at a temperature of from 1,950*-2,300*C to reoxidize any yttria that was reduced to yttrium during sintering. A dense body transparent to visible light is produced. If a transparent article is not desired, the purity can be reduced.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 10.
Claims (2 — 0 Independent, 2 Dependent)
- Claim 2Depends on #1
A method according to claim 1, wherein the heating step is carried out in a hydrogen atmosphere having a dew point of not higher than -20*C. at a temperature of from 2,200* to 2,300*C. for a period of time of not less than 60 minutes.
- Claim 3Depends on #1
A method according to claim 1, w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (2)
Non-Patent Literature (4)
- C. E. Curtis, Properties of Yttrium Oxide Ceramics , Jour. Amer. Cer. Soc., August, 1957, at 274 278
- J. D. Schieltz et al., Anomalous Sintering Behavior of Y O , Jour. Amer. Cer. Soc., August, 1967, at 439 440
- L. A. Brissette et al., Thermomechanically Deformed Y O , Jour. Amer. Cer. Soc., March, 1966, at 165 166
- L. R. Furlong et al., Sintering of Yttrium Oxide , Ceramic Bulletin, December, 1966, at 1,051 1,054