Patents
US 3,762,902 A#677028 Most CitedExpiredUnited States (USPTO)Utility

Shaping coating and tempering glass

59Forward Citations (#677028 Global)
1.1/yrCitation Velocity (#5682606 Global)
15.96Citation PageRank (#487068 Global)
0Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

Shaping, coating and tempering glass sheets in a continuous process comprising supporting a glass sheet in bending relation to a mold, heating the sheet in an enclosed atmosphere until it conforms to the mold, coating at least a surface of the bent sheet while so supported by applying a coating composition for a time sufficient to produce a coating thereon and while exposing its other surface to a cool atmosphere, discontinuing the coating before the glass temperature falls below the strain point, and then quenching both surfaces of the sheet rapidly with relatively cold tempering medium to impart at least a partial temper to the bent coated glass sheet before removing the sheet from the supporting mold. The temperature treatment can also simultaneously fuse a metalo-ceramic frit applied to a portion of the coated surface before said heating starts.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 59.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    The method as in claim 1, further including the step of applying to said surface of said glass sheet to be sprayed a stripe of a metalo-ceramic fusible frit capable of fusing to said glass sheet and forming a stripe of electroconductive material fused to said surface when subjected to said heating and chilling, said frit applying step being accomplished prior to said heating.

  2. Claim 3Depends on #2

    The method as in claim 2, wherein a pair of said stripes of fusible frit is applied along a pair of opposite side edges of said surface to be sprayed prior to said heating and chilling.

  3. Claim 4Depends on #1

    The method as in claim 1, wherein said elevated temperature is within the range of about 1,000* to about 1,300* Fahrenheit.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 59 total)

PatentTitleYearCitations
US 11,337,311 B2Aircraft window with variable power density heater film20220
US 11,509,132 B2Intelligent window heat control system20220
US 2004045320 A1Method for transporting glass panels through a coating installation and device for transporting said glass panels—2
US 2008011018 A1Device for transporting glazing through a coating-depositing plant—0
US 5,931,981 AProcess for quenching glass sheets with a cryogenic liquid and pressurized air19997
US 5,772,717 ATempering method using a two phase flow of cryogen19987
US 2010129533 A1Conductive Film Formation On Glass—4
US 10,202,302 B2Lithium containing glass with high and low oxidized iron content, and products using same20190
US 11,332,402 B2Tempering frame for thermal tempering of glass panes20220
US 7,645,314 B2Composition useful for making slow release nitrogen free phosphorous, potassium and sulfur oxide glass and a process of making glass therefrom20100
US 2006117823 A1Composition useful for making slow release nitrogen free phosphorous, potassium and sulfur oxide glass and a process of making glass therefrom—0
US 2005126225 A1Tumbled, polished, vibrated broken tempered glass pieces—5
US 9,384,601 B2Aircraft electronic fingerprint and monitoring performance of an aircraft component using the aircraft's electronic fingerprint20162
US 2002189086 A1Grounding assembly and method of producing same—5
US 11,150,389 B2Method of changing glass to high infrared absorbing glass having high oxidized iron content20210

References Cited — Backward Prior Art (0)

No backward patent references recorded.