Nickel aluminide coated low alloy stainless steel
Abstract
Low alloy austenitic stainless steel is protected from oxidative corrosion and erosion at high temperatures in the presence of exhaust gases from internal combustion engines by flame-spraying a layer between about 0.003 inches and about 0.007 inches thick of an alloy of 80 percent nickel and 20 percent chromium on the steel base, and thereafter converting the layer to an intermetallic chromium containing nickel aluminide coating by a low temperature aluminum cementation process. A cementation pack comprising 96 percent aluminum oxide, 2 percent aluminum, 1 percent sodium chloride, and 1 percent ammonium bifluoride is placed on the nickel-chromium layer in an inert atmosphere for a period between four hours and 24 hours at 1400*F to 1600*F to form an intermetallic chromium containing nickel aluminide coating containing 40 to 60 atomic percent aluminum. The coated steel is highly resistant to oxidation corrosion and erosion by high temperature exhaust gases from internal combustion engines. It is particularly useful in the construction of thermal reactors for exhaust systems in automobiles for the control of pollution from exhausts.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 29.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
An article of manufacture as claimed in claim 1 wherein said coating is produced by applying aluminum by means of low temperature pack cementation to a flame-sprayed layer between about 0.003 inch and about 0.007 inch thick of 80 percent nickel-20 percent chromium alloy on said base, said aluminum reacting with said layer to form said nickel aluminide.
- Claim 3Depends on #2
An article of manufacture as claimed in claim 2 wherein said austenitic stainless steel is a low nickel alloy stainless steel, and said aluminum is applied from a cementation pack comprising 96 percent aluminum oxide, 2 percent aluminum, 1 percent sodium chloride, and 1 percent ammonium bifluoride.
- Claim 4Depends on #2
An article of manufacture as claimed in claim 2 wherein said aluminum is applied in an inert atmosphere at about 1400* to 1600*F.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 29 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.