Austenitic alloy containing boron and processes for manufacturing thesame
Abstract
An austenitic ferrous base alloy characterized by improved stability at high temperatures, and by improved resistance to sensitization and to corrosion, cracking, and general deterioration. The austenite is an iron-chromium-nickel alloy containing from 0.01 to 0.2 percent boron, less than 0.009 percent carbon, and substantially free from nitrogen and oxygen. The boron is a solute in the austenite. The process of manufacture is to form a melt of iron, chromium, nickel and other additives, and then add a ferro-boron alloy having a melting point well below that of the base alloy. The process is carried out in a vacuum furnace in order to substantially eliminate carbon, nitrogen, and oxygen from the alloy.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 2Independent Claim
A ferrous base alloy characterized by high temperature stability and by being substantially completely austenitic, consisting essentially of from about 12 percent to about 30 percent by weight cHromium, from about 8 percent to about 20 percent by weight nickel, from about 0.01 percent to about 0.2 percent boron, 0 percent to about 2.5 percent by weight manganese, 0 percent to about 1.5 percent by weight silicon, less than 0.009 percent by weight carbon, and in which the total amount of carbon and nitrogen is less than 0.01 percent by weight, and the balance iron with incidental impurities that
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.