Patents
US 3,753,682 A#10029329 Most CitedExpiredUnited States (USPTO)Utility

Ported rotary kiln process for direct reduction of oxides of metallic minerals

10Forward Citations (#10029329 Global)
0.2/yrCitation Velocity (#34509865 Global)
2.77Citation PageRank (#8607729 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process is disclosed for prereducing metallic oxide and sulfide ores to a lower state of oxidation without passing through a liquid phase, at an accelerated rate. The ore particles are preheated to 1,800* or above. An unreformed hydrocarbon fuel such as natural gas (CH4) substantially free of any oxidizing agents is passed into a bed of such preheated ore particles to pyrolytically decompose and reform portions of the fuel into strong reducing agents while in intimate contact with the oxidic metal to be reduced. Such forming of reducing agents cause at least some ore to very quickly reduce to a lower state of oxidation with an attendant solid state reorientation of metal and/or sulfur and oxygen atoms. The atomic reorientation provides increased porosity, and greater surface area is exposed to the strong reducing agents for additional and continued reduction. Portions of as yet unreformed fuel in the bed are rapidly reformed by continued pyrolysis and by reacting with oxygen and/or sulfur from the ore, to provide additional quantities of strong reducing agents.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    A process according to claim 1 in which the charge of lumps or agglomerates is heated to at least a temperature level of about 1,922* to 2,000* F before being charged to the kiln zone provided with porting means.

  2. Claim 3Depends on #1

    A process according to claim 1 in which the charge of lumps or agglomerates is prepared to include particles of solid carbonaceous material; and during the heating of the charge before being charged to the ported zone, carbonaceous material within the charge is oxidized by reacting with the lumps or agglomerates of material to partially reduce the lumps or agglomerates before being charged to the ported zone.

  3. Claim 4Independent Claim

    A process for directly reducing iron oxide ore without melting to a metalization of 90 percent or more in a generally horizontal rotary kiln, comprising the steps of: a. heating a charge of lumps or agglomerates of fines of i

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗