US 3,735,971 A#4017364 Most CitedExpiredUnited States (USPTO)Utility

Strainable members exposed to temperature variations and materials therefor

21Forward Citations (#4017364 Global)
0.4/yrCitation Velocity (#19653452 Global)
2.56Citation PageRank (#9794240 Global)
2Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

A temperature-stable strainable member is formed of an antiferromagnetic alloy having a low temperature-coefficient of the modulus of elasticity. The member may be embodied in a mechanical oscillator as a vibratory element with a modulus of elasticity whose temperature coefficient is between -10 . 10 5 and +10 . 10 5 centigrade and which is composed of 20 - 29 percent manganese, 2 - 9 percent chromium, 0.03 - 1 percent carbon, the remainder iron with ordinary impurities less than 1 percent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 21.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A system as claimed in claim 1, wherein said third portion comprises 20 to 29 percent Mn, 2 to 9 percent X, 0.03 to 1 percent Y, 0 to 1.5 percent Al, Be, Ti, Nb, with the remainder Fe and impurities below 1 percent, wherein X is Cr + Ni + Co + V + Mo + W + Si but Ni + Co + V + Ro + W + Si only from 0 to 4 percent, and wherein Y is C + N but N only from 0 to 0.3 percent.

  2. Claim 3Depends on #2

    A system as claimed in claim 2, wherein the weight percentages %Mn +(0.6 X % X)-(5.0 X % Y) 21 to 27.

  3. Claim 4Depends on #2

    A system as claimed in claim 2, wherein the weight percentages % Mn +(0.6 X % Cr)-(5.0 X %C) 21 to 27.