Patents
US 3,725,533 A#5029557 Most CitedExpiredUnited States (USPTO)Utility

Boron carbide fiber production

18Forward Citations (#5029557 Global)
0.3/yrCitation Velocity (#22532768 Global)
2.26Citation PageRank (#11949927 Global)
2Prior Art Cited
3Claims (0 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

Boric oxide fibers having a maximum diameter of about 10 microns are heated in an ammonia atmosphere to about 350*-600*C at a rate of temperature rise of up to about 5,000*C/hr. to produce ammonia-treated fibers consisting essentially of B, N. O and H. The ammonia-treated fibers are heated in an amine atmosphere at about 600*-1,000*C to produce amine-treated fibers consisting essentially of B, C, N, O and H and containing at least about 15% C. The amine-treated fibers may be heated at about 2,000*-2,350*C in an inert atmosphere to produce boron carbide fibers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 18.

Claims (3 — 0 Independent, 3 Dependent)

  1. Claim 2Depends on #1

    A process as set forth in claim 1 wherein said heating in an ammonia atmosphere is begun at a starting temperature below about 250*C.

  2. Claim 3Depends on #2

    A process as set forth in claim 2 wherein said rate of temperature rise is at least about 5*C/hr.

  3. Claim 4Depends on #2

    A process as set forth in claim 2 wherein said rate of temperature rise is between about 10*C/hr. and about 100*C/hr.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)

Non-Patent Literature (1)

  • Conroy et al., Proceedings Of The Third Conference On Carbon, pages 395 403 (1959)