Amorphous polypropylene stabilized hot melt adhesive
Abstract
Hot melt adhesive compositions with resistance to crusting and stable viscosity characteristics are prepared from a mixture of ethylene-vinyl acetate copolymer, glycerol ester of hydrogenated rosin, wax, and amorphous polypropylene. The improved hot melt adhesive formulation can contain from about 30 to about 50 percent by weight ethylene-vinyl acetate copolymer, from about 20 to about 40 percent by weight of glycerol ester of hydrogenated rosin, from about 20 to about 40 percent by weight of a wax, and from about 10 to about 30 percent by weight amorphous polypropylene.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 31.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A hot melt adhesive composition comprising (1) about 10 to about 30 percent by weight amorphous polypropylene having a molecular weight of less than 10,000; (2) about 20 to about 40 percent by weight of a wax; (3) about 20 to about 40 percent by weight of a rosin tackifier and (4) about 30 to about 50 percent by weight of an ethylene-vinyl acetate copolymer.
- Claim 2Depends on #1
The hot melt adhesive composition of claim 1 wherein an antioxidant formulation in the range of up to 0.5 percent by weight of the total weight of the formulation is present in the composition.
- Claim 3Depends on #1
A hot melt adhesive composition of claim 1 wherein the amorphous polypropylene has a molecular weight in the range of 7, 000 to 8,000 and has a crystallinity of less than 5 percent.
Technical Overview & Description