Abstract
A hard solder contains: 27-40 wt.% Mn, 11-20 wt.% Ni, 7-15 wt.% Cu, 0.5-4.5 wt.% Si , 0.02-0.5 wt.% C, 0.05-0.5 wt.% B, 0.03-10.5 wt.% Al, S and P together not in excess of 0.08 wt.%, Fe being the balance, the solder in view of the composition thereof enabling an equal-strength brazing joint to be obtained.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 1.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
A solder as claimed in claim 1, which incorporates said components in the following weight percentage: 32.0 Mn, 12.5 Ni, 12.0 Cu, 2.5 Si, 1.0 C, 0.07 B, 0.03 Al, S and P together not in excess of 0.05, Fe being the balance.
- Claim 3Depends on #1
A solder as claimed in claim 1, which apart from the afore-mentioned components also contains also Sb up to 3.5 wt. percent, all the remaining components being taken in the following weight percentage:32.0 Mn, 12.5 Ni, 12.0 Cu, 2.5 Si, 1.0 C, 0.08 B, 0.03 Al, S and P together not in excess of 0.06, Fe being the balance.
- Claim 4Depends on #1
A solder as claimed in claim 1, wherein Mn and Si are contained in the form of double and triple solid solutions with Fe, Ni and Cu.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,202,687 A | Low melting point Ni-Cr alloy for cast dental products | 1980 | 2 |
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,856,281 A | High temperature brazing alloys | 1958 | 42 |
| US 3,516,825 A | Solder for soldering or brazing cast iron | 1970 | 11 |