Patents
US 3,708,352 A#11213388 Most CitedExpiredUnited States (USPTO)Utility

Strain hardened aluminum-magnesium alloys

9Forward Citations (#11213388 Global)
0.2/yrCitation Velocity (#35945189 Global)
2.71Citation PageRank (#8905927 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

ALUMINUM ALLOY PLATE CONTAINING 4.4 TO 10% MAGNESIUM AND STRAIN HARDENED TO IMPROVE ITS STRENGTH TO A LEVEL OF AT LEAST 40% GREATER THAN THE STRENGTH IN THE ANNEALED STATE IS IMPARTED WITH SUBSTANTIALLY FREEDOM FROM SUSCEPTIBILITY OF EXFOLIATION CORROSION. THE PROCESS INCLUDES ROLLING AT MINIMUM TEMPERATURES OF ABOUT 420* TO 650*F. DEPENDING ON THE AMOUNT OF MAGNESIUM PRESENT, TO PRODUCE THE STRAIN HARDENED PRODUCT AND COOLING AT SPECIALLY CONTROLLED RATES.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.