Patents
US 3,707,901 A#2415049 Most CitedExpiredUnited States (USPTO)Utility

Pavement and composition therefor

29Forward Citations (#2415049 Global)
0.6/yrCitation Velocity (#14483437 Global)
3.94Citation PageRank (#4889822 Global)
8Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Pavement having an inner layer between a surface course and a base, and a composition therefor. The inner layer may comprise ground tire stock or other particulate vulcanized rubber together with sand or other fine material aggregate, and, as a binder, asphalt from an oil-in-water asphalt emulsion which may be about 65 percent asphalt. A typical composition may contain equal parts by volume of mineral aggregate and particulate vulcanized rubber, and asphalt emulsion in an amount of 20 to 40 percent of the total volume. The layer, which may be from about one-eighth to one-half inch in thickness, will serve to relieve strain in the surface course and to arrest cracking thereof, by virtue of its reduced elastic modulus. In addition, it will desirably fill cracks in the base, and protect the base.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 29.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 2Depends on #1

    A pavement as in claim 1 wherein the inner layer comprises ground vulcanized rubber substantially 100 percent of which will pass a one-quarter inch screen at least half of which will be retained on a No. 8 screen, and substantially 0 percent of which will pass a No. 50 screen, and fine mineral aggregate substantially 100 percent of which will pass a No. 4 screen.

  2. Claim 3Independent Claim

    A pavement composition relieving strain and arresting cracks in pavements consisting essentially, by volume, of from 30 to 50 percent of ground vulcanized rubber, from 20 to 40 percent of fine mineral aggregate, and from 15 to 35 percent of residual asphaltic binder from an emulsion, and reacting visco-elastically when subjected to relatively low rates of strain and elastically when subjected to relatively high rates of strain, the ground vulcanized rubber being of a size such that substantially 100 per

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗