Production of molds
Abstract
A method of producing precision casting molds from a mixture of a comminuted refractory material, a lower alkyl silicate binder and a gelling accelerator. The proportion of lower alkyl silicate used, and the mean effective particle size and particle size distribution of the refractory are both carefully controlled. Specifically, the proportion of lower alkyl silicate used is kept sufficiently low that the mixture, when placed against a pattern and allowed to gel, does not crack upon prolonged standing under ambient conditions, while a refractory is used substantially all of which is finer than 8 mesh and in which the particle size is graduated so that a substantial proportion is finer than 200 mesh and a substantial proportion is coarser than 100 mesh, while the bulk density is sufficiently high that, at the required low proportion of alkyl silicate, the mixture can be placed in moldforming relationship with a pattern and, upon gelling of the alkyl silicate, will form a rigid mold. Apart from control of the proportion of lower alkyl silicate used and of particle size of the refractory, the process is conventional, and involves producing the mixture, applying the mixture in mold-for
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 5.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
In a method as claimed in claim 1, the improvement wherein the pattern is separated from the slurry after gellation thereof to a rigid condition.
- Claim 3Depends on #1
In a method as in claim 1, the improvement of using not more than 23 ml of the lower alkyl silicate binder per 100 gm. of the particulate refractory composition so that the mold, before firing, does not crack upon prolonged standing under ambient conditions, and of using as the refractory a blend of 30 parts of minus 200 mesh wollastonite and 70 parts of wollastonite having the following particle sizing: plus 20 mesh screen 22.6 minus 20 plus 45 mesh screen 46.4 minus 45 plus 100 mesh screen 22.4 minus 100 plus 200 mesh screen 7.1 minus 200 mesh screen 1.5
- Claim 4Depends on #1
In a methOd as in claim 1, the improvement of using not more than 12.5 ml. of the lower alkyl silicate binder per 100 gram of the refractory c