US 3,680,197 A#6038504 Most CitedExpiredUnited States (USPTO)Utility

Diffusion bonding method

15Forward Citations (#6038504 Global)
0.3/yrCitation Velocity (#27040054 Global)
5.28Citation PageRank (#3033944 Global)
7Prior Art Cited
2Claims (0 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A diffusion bonding method for the alloys exhibiting a defined recrystallization temperature, or eutectoid or peritectoid behavior as part of their phase equilibrium characteristics, which involves repetitively cycling the alloy to be joined between a temperature slightly above and below the recrystallization temperature, or allotropic transformation temperature, and controlling the rate of new grain nucleation and growth across the joint interface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 15.

Claims (2 — 0 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    The method according to claim 1 wherein; the closure pressure does not exceed that providing a tolerable deformation at the bonding temperature.

  2. Claim 3Depends on #1

    The method according to claim 1 wherein; subsequent to the bonding step, the bonded alloys at the interface are normalized or homogenized by heat treatment.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗