Hydroconversion catalyst preparation
Abstract
Incorporation of 30-65 percent of a hydrogenation metal component into a hydrogel which would yield on drying and calcining without the hydrogenation metals a xerogel of a high compacted bulk density (0.8-1.6 g/cc) low pore volume (0.15-0.45 cc/g.) alumina results in a catalyst having a very high hydrogenation and dentrification activity. Up to about 10 percent fluoride is added to provide a cracking component. The hydrogenation metal component is selected from the oxides of nickel, molybdenum, tungsten, cobalt and mixtures thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 18.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The method of claim 1 wherein the hydrogel is washed to remove extraneous counter ions before contacting with the metal salt solution at a temperature from 60* to 250* C.
- Claim 3Depends on #1
The method of claim 1 wherein from 1 to 9 percent wt. fluoride is incorporated into the composite.
- Claim 4Depends on #1
The method of claim 1 wherein after the contact with metal salt solution the hydrogel is shaped and partially dried to remove about 3 to 60% wt. of the water content then washed to remove extraneous counter ions.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗