Process for producing electrode binder pitch and carbon black feedstock
Abstract
There is disclosed a process for converting the residue portion of a cracked petroleum product into electrode binder pitch and carbon black feedstock, both more valuable products, by heat soaking the residue to produce electrode binder pitch and a middle distillate, and blending the middle distillate with some of the electrode binder pitch to produce a carbon black feedstock.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 15.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The process of claim 1 wherein the residual fraction separated from the cracked product has an initial boiling point between 250* and 400* C.
- Claim 3Depends on #1
The process of claim 1 wherein the heat soaking is carried out under a pressure above atmospheric at a temperature between 400* and 450* C. for 2 hours at most.
- Claim 4Depends on #1
The process of claim 1 wherein the heat soaking is carried out at a temperature between 350* and 400* C., while air is passed through the liquid.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,752,290 A | Production of pitch from petroleum residues | 1956 | 23 |
| US 2,992,181 A | Process for producing a petroleum base pitch | 1961 | 22 |
| US 3,412,009 A | Process for producing carbon black oil | 1968 | 11 |