Polyethylene terephthalate films containing hydrated aluminum silicate for less shrinkage and abrasion
Abstract
A polyethylene terephthalate film is produced having improved abrasion resistance and low shrinkage properties by the dispersing in the film of hydrated aluminum silicate. The improved film has a coefficient of friction in the range of 0.3 to about 1.0 and the hydrated silica ranges from 0.01 percent to about 0.5 percent by weight of the polymer and has a particle size from about 300 to 1000 millimicrons. The film has an intrinsic viscosity of 0.2 to about 1.0 and after biaxially stretching is heated at 215* C. - 235* C. for a period of time to complete crystallization.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 17.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The method of claim 1 wherein the film is biaxially stretched from about 2.5 to about 4.0 times its original dimensions.
- Claim 3Depends on #2
The method of claim 2 wherein the hydrated aluminum silicate as dispersed ranges in amounts from about 0.05 to about 0.3 percent by weight of the total polymer.
- Claim 4Depends on #3
The method of claim 3 wherein the intrinsic viscosity of the polymer ranges from about 0.4 to about 1.0 deciliters per gram.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (2)
- Grant, Julius, A Laboratory Handbook of Pulp and Paper Manufacture, Longmans Green & Co., 1942 New York City, frontispiece and pages 115, 116.
- Modern Plastics Encyclopedia 1967, the September issue of Modern Plastics, 1966, Vol. 44, No. 1A, McGraw Hill New York City, frontispiece and pages 590, 591, 592.